Instructions

 

1. Characteristics of base material: the base material must be clean, dry and free of oil stain and release agent. Use alcohol or special solvent to scrub or soak the surface of equipment.

 

2. Mixing and dilution: before use, it must be stirred evenly to ensure that there is no precipitation. Normal use does not need to be diluted. If it needs to be diluted, it can be diluted to the viscosity required by the construction with boiled oil. The recommended dilution ratio is 2 parts of oil and 1 part of diluent (i.e. 2:1).

 

3. Spraying: spray gun form w-71, caliber 0.5 – 2mm

 

Distance between spray gun and object: 100 – 200mm

 

Spraying air pressure 0.4 – 0.6MPa

 

Spraying amount 2-4 circulation film thickness 15-25 μ M

 

4. Anti sedimentation operation: small workpieces shall be sprayed with 2-3 guns once, and oil shall be stirred once every 3-4 guns; large workpieces shall be sprayed with 1 gun once, and oil shall be stirred once every 4-5 guns

 

5. Drying: natural drying (25 ℃) surface drying for 5 minutes / solid drying for 2 hours; drying at 65 ℃ for 20 minutes, after drying for 1 hour, the best resistance can be obtained.

 

 

 

 

Safety and storage

 

1. Keep away from heat and fire. Taboo: spark, open fire, high temperature.

 

2. Please read the manual carefully before use.

 

3. Pay attention to the operation, avoid direct contact with skin or eyes, and prepare for protection.

 

4. Store at room temperature for 6 months (original barrel).